Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.400 - 26.9 g/10 min | 0.400 - 26.9 g/10 min | Average value: 4.70 g/10 min Grade Count:13 |
Overview of materials for Styrene/Methyl Methacrylate Copolymer (SMMA) This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Methyl Methacrylate Copolymer (SMMA)". Each property range of values reported is minimum and max.. |