Polymer Property : Melt Flow = 26.4 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 26.4 g/10 min

@Load 5.00 kg,
Temperature 260 °C
26.4 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ASTM D1238
Diamond Polymers DIAMALOY 527 PC/PBT Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 26.4 g/10 min

@Load 14.91 kg,
Temperature 175 °C
26.4 g/10 min

@Load 32.87 lb,
Temperature 347 °F
ASTM D-1238
Axiall 1751 Clear 7002 Flexible PVC
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation ..