Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Melt Flow = 25.2 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 25.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
25.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® BPL1000 PC
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Melt Flow 25.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
25.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® BPL1000 PC (Asia Pacific)
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Melt Flow 25.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
25.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® BPL1000 PC (Europe-Africa-Middle East)
Lexan* BPL1000 Polycarbonate (PC) resin is an injection moldable grade featuring high flow and good impact peroformance. It contains non-chlorinated and non-brominated flame retardant systems with U..
Melt Flow 25.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
25.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Calculated from Volume Flow Rate of 21 cm<sup>3</sup>/10min.; ISO 1133
Mitsubishi Xantar® MX 1001 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Melt Flow 25.2 g/10 min

@Load 1.20 kg,
Temperature 300 °C
25.2 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Calculated from Volume Flow Rate of 21 cm<sup>3</sup>/10min.; ISO 1133
Mitsubishi Xantar® MX 1002 Polycarbonate
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Melt Flow 25.2 g/10 min

@Load 2.16 kg,
Temperature 300 °C
25.2 g/10 min

@Load 4.76 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics LNP THERMOCOMP D351 PC (Asia Pacific)
LNP* Thermocomp* D351 (experimental grade name as EXTC8143) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus,..
Copyright © lookpolymers.com All Rights Reserved