Polymer Property : Melt Flow = 240 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 160 - 240 g/10 min
160 - 240 g/10 min
PTM-008
Westlake Epolene® C-13 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer
Product Description: Epolene C-13 is a branched low density polyethylene homopolymer with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color conc..
Melt Flow 160 - 240 g/10 min
160 - 240 g/10 min
72-412
Westlake Epolene® C-13P Coating Grade - Branched Medium Molecular Weight Polyethylene Polymer
Description: Epolene C-13P is a branched low density polyethylene homopolymer powder with low color and medium molecular weight. It is useful as a base polymer for adhesives and coatings, color con..