Polymer Property : Melt Flow = 24.48 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 24.48 g/10 min

@Load 1.20 kg,
Temperature 300 °C
24.48 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Lehmann & Voss LUVOCOM® 50-8479/BL-1 Polycarbonate, unreinforced
Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Isotropic shrinkage characteristics.Reduced moment of inertia ..