Melt Flow 3.00 - 236 g/10 min
3.00 - 236 g/10 min
Average value: 35.8 g/10 min Grade Count:92
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Melt Flow 9.50 - 236 g/10 min
9.50 - 236 g/10 min
Average value: 41.6 g/10 min Grade Count:18
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an..