Polymer Property : Melt Flow = 236 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 236 g/10 min

@Load 2.16 kg,
Temperature 250 °C
236 g/10 min

@Load 4.76 lb,
Temperature 482 °F
Estimated using room temperature density; ISO 1133
Lanxess Pocan® B 700 000000 PBT  (discontinued **)
PBT, non-reinforced, extrusion, improved flowability