Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 20.2 g/10 min | 20.2 g/10 min | ISO 1133 |
Solvay Engineered Polymers SEQUEL® 5220 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 5220 engineered polyolefin is designed for large exterior applications that require superior painted gouge/scuff performance. This product also offers ductile impact propertie.. |
|||
Melt Flow | 20.2 g/10 min | 20.2 g/10 min | |
Kraton® G1657 + PP blend + Talc (12/21/67) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Melt Flow | 20.2 g/10 min @Load 5.00 kg, Temperature 280 °C |
20.2 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Melt Flow | 20.2 g/10 min @Load 5.00 kg, Temperature 280 °C |
20.2 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Europe-Africa-Middle East) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |
|||
Melt Flow | 20.2 g/10 min @Load 5.00 kg, Temperature 280 °C |
20.2 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL WCV065 PPE+Polyolefin (Asia Pacific) Flexible, non-halogenated FR, PPE+Polyolefin resin designed for evaluation in Automotive ISO6722 Class A-C applications. |