Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1020 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for molding flexible articles. Examples: fittings, rail pads, medical.ISO data provided by the manufacturer, Arkema. |
|||
Melt Flow | 2.55 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.55 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1020 VG 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high mechanical properties. Examples: films, chemical bags, gloves.ISO data provided by the manufactur.. |