Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.45 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-1003 NT 7 is an ethylene-hexene-1 copolymer, design.. |
|||
Melt Flow | 2.45 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.45 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-1003 NT 7 is an ethylene-hexene-1 copolymer, design.. |