Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 19.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
19.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer Improved flow PC with excellent processability and mold release. |
|||
Melt Flow | 19.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
19.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LyondellBasell Alathon® H4620 High Density Polyethylene, Injection Molding Grade Alathon H4620 is a medium-flow resin that exhibits good cold temperature impact performance, enhanced processing and thermal stability. Typical applications are thinner-walled parts that require che.. |
|||
Melt Flow | 19.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
19.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 50-7897 Polycarbonate, with PTFE Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Melt Flow | 19.5 - 20.5 g/10 min @Load 2.16 kg, Temperature 250 °C |
19.5 - 20.5 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
GRECO ISOPAK 640 Polycarbonate/ABS Alloy Flame retardant polycarbonate/ABS alloy; good impact and dimensional stabilityInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Melt Flow | 19.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
19.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical XG568 MABS, Anti-Scratch, High Gloss Feature: Injection Molding, Anti-Scratch, High GlossApplication: LCD TV Front Cabinet, Bezel, Audio/Video HousingCSA No. 9011-14-7 and 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 19.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
19.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 123X PC Copolymer (Asia Pacific) Improved flow PC with excellent processability and mold release. |