Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 18.7 g/10 min | 18.7 g/10 min | ISO 1133 |
Tisan TISETILEN® UNR Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |