Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 18.48 g/10 min @Load 5.00 kg, Temperature 190 °C |
18.48 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Lehmann & Voss LUVOCOM® 80/CF/12/TF/10/GY Polyacetal-copolymer, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |