Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 18.15 g/10 min @Load 5.00 kg, Temperature 235 °C |
18.15 g/10 min @Load 11.0 lb, Temperature 455 °F |
ISO 1133 |
BASF Ultramid® TG3S BK 5966 15% Glass Filled PA6 (Dry) Description: Ultramid TG7S Bk-102 is a 34% glass reinforced, pigmented black, heat stabilized, impact modified PA6 injection molding grade. It was developed to meet the demanding requirements of the.. |