Physical Properties Metric English Comments
Melt Flow 18.0 g/10 min

@Load 1.20 kg,
Temperature 300 °C
18.0 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D123
Niche Polymer PCM18BK PC
Information provided by Niche Polymer
Melt Flow 18.0 - 24.0 g/10 min

@Load 1.106 kg,
Temperature 300 °C
18.0 - 24.0 g/10 min

@Load 2.439 lb,
Temperature 572 °F
ASTM D1238
Oxford Polymers PC C20-000 Clear PC
Product Description: Amorphous, Unreinforced Polycarbonate injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Pigment onlySpecial Characteristics: Easy fl..
Melt Flow 18.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP 1249B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP 2104 Thermoplastic Elastomer
Features: Nice Silken Feel Uses: Safety ProductsInformation Provided by Teknor Apex
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1625A Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-1671 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2111S-L3 Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Monprene® MP-2815B Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 18.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Monprene® MP-2840M Thermoplastic Elastomer
Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo..
Melt Flow 18.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® 90-E607B-75NT Ethylene Vinyl Acetate Copolymer
Notes: The Specialty Compounding Division offers a proprietary line of cap-liner compounds designed for carbonated soft drinks. These are proven products that have been used commercially for several..
Melt Flow 18.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-1431F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-1934A BLK 111 Thermoplastic Elastomer
Information Provided by Teknor Apex
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection..
Melt Flow 18.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2625C Thermoplastic Elastomer
Uses: Consumer Applications; General Purpose; Gaskets; Handles; Personal Care; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Ext..
Melt Flow 18.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
18.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Telcar® TL-2519F Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex Elexar® EL 1446A Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical properti..
Melt Flow 18.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
18.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238