Physical Properties Metric English Comments
Melt Flow 16.9 g/10 min

@Load 1.20 kg,
Temperature 300 °C
16.9 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133:1997
Nanocyl PLASTICYL™ PC1501 Polycarbonate with 2 wt% Multi-Wall Carbon Nanotubes
PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA..
Melt Flow 16.9 g/10 min

@Load 10.0 kg,
Temperature 250 °C
16.9 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL INT1001 PPE+HIPS (Asia Pacific)
PPE / HIPS unfilled, high flow for auto interior