Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16.72 g/10 min @Load 5.00 kg, Temperature 250 °C |
16.72 g/10 min @Load 11.0 lb, Temperature 482 °F |
|
Lehmann & Voss LUVOCOM® 1850-7581 PBT, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |