Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 16.05 g/10 min @Load 10.0 kg, Temperature 220 °C |
16.05 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® S 777 K UV Black 56625 ASA Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |