Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 15.69 g/10 min @Load 5.00 kg, Temperature 200 °C |
15.69 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution Polystyrol 145 D PS Description: Polystyrol 145 D is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol.Applications: In blends with high impact polystyrene esp.. |