Physical Properties Metric English Comments
Melt Flow 12.1 - 15.3 g/10 min
12.1 - 15.3 g/10 min
Average value: 14.1 g/10 min Grade Count:3
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..