Polymer Property : Melt Flow = 145 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 145 g/10 min

@Load 5.00 kg,
Temperature 275 °C
145 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3S Q661 PA6 (Dry)
Ultramid B3S Q661 is a general purpose, PA6 resin for injection molding.