Physical Properties Metric English Comments
Melt Flow 14.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Plastcom PLASTAMID® 6 BT N 29 B/IM PA6
Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natu..
Melt Flow 14.5 g/10 min

@Load 2.16 kg,
Temperature 260 °C
14.5 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Asia Pacific)
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 920 PC
Opaque colors, low viscosity, superior flame retardance.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 920 PC (Asia Pacific)
Opaque colors, low viscosity, superior flame retardance.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 920A PC
Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 923 PC
Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 923 PC (Asia Pacific)
Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 923A PC
Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific)
Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 923ASR PC
More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance.
Melt Flow 14.5 g/10 min

@Load 2.16 kg,
Temperature 260 °C
14.5 g/10 min

@Load 4.76 lb,
Temperature 500 °F
ASTM D1238
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS
Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific)
Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® 920ASR PC
More robust design of standard 900 series flame retardant grade. Internal mold release.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance.
Melt Flow 14.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
14.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Asia Pacific)
This product will be phased out per January 2015 -- Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance.
Melt Flow 14.5 g/10 min

@Load 5.00 kg,
Temperature 230 °C
14.5 g/10 min

@Load 11.0 lb,
Temperature 446 °F
ISO 1133
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer
INNOPOL® CS 1-5140 BLH is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-5140 BLH is recommended especially for producing products, where high stiffn..
Melt Flow 14.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D 1238
Styrolution PS 5801 HIPS
Exceptional processabilityHigh toughnessUSP Class VI certifiedUl Classification 94 HBInformation provided by Styrolution
Melt Flow 14.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Dow TF0807 TPO
Dow Fascia TPO for Painted ApplicationsInformation provided by Dow
Melt Flow 14.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
DIN 5375/ISO 1133
Ineos Nova S-3201 Medium Impact Compact Polystyrene  (discontinued **)
Extremely easy flowing medium impact polystyrene, designed for extreme short cycle times for injection molding of household, packaging and toys. The material is provided with external lubricant to ..
Melt Flow 14.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
14.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Ineos H14A-00 Polypropylene Homopolymer
Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,..