Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | <= 14.3 g/10 min @Load 10.0 kg, Temperature 380 °C |
<= 14.3 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-7781 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Melt Flow | <= 14.3 g/10 min @Load 2.16 kg, Temperature 300 °C |
<= 14.3 g/10 min @Load 4.76 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® PA66/TF/40 Polyamide 66, with PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Melt Flow | 14.3 g/10 min @Load 10.0 kg, Temperature 380 °C |
14.3 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-8339 PEEK, lubricant modified Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Chemical and hydrolysis resistance parts, non flammable.Improved friction and wear behavio.. |