Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.53 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.53 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 11 cm<sup>3</sup>/10 min; ISO 1133 |
DSM Arnitel® PL581 58 Shore D, Injection Grade Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 13.53 g/10 min @Load 2.16 kg, Temperature 230 °C |
13.53 g/10 min @Load 4.76 lb, Temperature 446 °F |
Calculated from Volume Flow Rate of 11 cm<sup>3</sup>/10min.; ISO 1133 |
DSM Arnitel® PL581 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |