Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.3 g/10 min @Load 5.00 kg, Temperature 300 °C |
13.3 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL CN5260 PPE+PS (Asia Pacific) 50% filled FR high modulus PPE/PS blend |
|||
Melt Flow | 13.3 g/10 min @Load 3.80 kg, Temperature 230 °C |
13.3 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Arkema Group Oroglas® VM Acrylic, Injection Molding Grade
(discontinued **) OROGLAS VM is an injection molding grade with a medium heat resistance and easy flow.OROGLAS VM is particularly suitable to improve mold filling of technical parts.The VM L version has been speciall.. |