Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.22 g/10 min @Load 1.20 kg, Temperature 300 °C |
13.22 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133:1997 |
Nanocyl PLASTICYL™ PA1501 Polyamide 66 with 3 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |