Polymer Property : Melt Flow = 127 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 127 g/10 min

@Load 1.20 kg,
Temperature 250 °C
127 g/10 min

@Load 2.65 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® 175 PBT (Europe-Africa-Middle East)
Unreinforced, neat PBT resin for compounding only. Natural Color Only, Not intended for injection molding.
Melt Flow 127 g/10 min

@Load 1.20 kg,
Temperature 250 °C
127 g/10 min

@Load 2.65 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® 176 PBT
Unreinforced, neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.
Melt Flow 127 g/10 min

@Load 1.20 kg,
Temperature 250 °C
127 g/10 min

@Load 2.65 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® 176HP PBT
Unreinforced, FDA compliant neat PBT resin for fibers. Natural Color Only, Not intended for injection molding.