Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 125 g/10 min @Load 2.16 kg, Temperature 230 °C |
125 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HK060AE Polypropylene Homopolymer HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr.. |
|||
Melt Flow | 125 g/10 min @Load 2.16 kg |
125 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 6.5. |
Dow DOWLEX™ 2503.10 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2503.10 Polyethylene resin is a narrow molecular weight distribution copolymer designed as a superior processing resin. For very thin wall higher cavitation molding, this grade often is a p.. |
|||
Melt Flow | 125 g/10 min @Load 14.91 kg, Temperature 175 °C |
125 g/10 min @Load 32.87 lb, Temperature 347 °F |
ASTM D-1238 |
Axiall 1601 Clear 7002 Flexible PVC Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation .. |