Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.00 - 121 g/10 min | 3.00 - 121 g/10 min | Average value: 33.7 g/10 min Grade Count:25 |
Overview of materials for Nylon 6, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Impact Grade". Each property range of values reported is minimum and maximum values of appropri.. |