Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12.84 g/10 min @Load 10.0 kg, Temperature 220 °C |
12.84 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® S KR 2859 ASA Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Melt Flow | 12.84 g/10 min @Load 10.0 kg, Temperature 220 °C |
12.84 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® S KR 2859 UV ASA Description: Stiff extrusions product, versatile grade for profile and sheet extrusion as protective cap layer.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |