Melt Flow 12.7 g/10 min

@Load 5.00 kg,
Temperature 250 °C
12.7 g/10 min

@Load 11.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics Valox® 337 PBT
Low temperature impact PBT. Automotive applications: underhood power distribution boxes and covers.