Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 104 g/10 min @Load 2.16 kg, Temperature 250 °C |
104 g/10 min @Load 4.76 lb, Temperature 482 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® B 1100 000000 PBT PBT, non-reinforced, extrusion, injection molding, improved flowability |