Polymer Property : Melt Flow = 10.8 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 10.8 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.8 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East)
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..
Melt Flow 10.8 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.8 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® ML4506 PC
Transparent polycarbonate for aircraft applications requiring FAR 25.853a compliance. Injection moldable.
Melt Flow 10.8 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.8 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
SABIC Innovative Plastics Lexan® FXM141R PC (Asia Pacific)
FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color ..
Melt Flow 10.8 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.8 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Calculated from Volume Flow Rate of 8 cm<sup>3</sup>/10min.; ISO 1133
Mitsubishi Xantar® G4F 22 R Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Melt Flow 10.8 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10.8 g/10 min

@Load 2.65 lb,
Temperature 572 °F
Calculated from Volume Flow Rate of 8 cm<sup>3</sup>/10min.; ISO 1133
Mitsubishi Xantar® G4F 22 UR Polycarbonate-20% Glass Reinforced
Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances ..
Melt Flow 10.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Calculated from Volume Flow Rate of 9 cm<sup>3</sup>/10 min; ISO 1133
DSM Arnitel® PM471 45 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melt Flow 10.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Calculated from Volume Flow Rate of 9 cm<sup>3</sup>/10min.; ISO 1133
DSM Arnitel® PM471 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..