Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.6 g/10 min @Load 5.00 kg, Temperature 260 °C |
10.6 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
Melt Flow | 10.6 g/10 min @Load 5.00 kg, Temperature 260 °C |
10.6 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |
|||
Melt Flow | 10.6 g/10 min @Load 5.00 kg, Temperature 275 °C |
10.6 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
BASF Ultramid® A3Z BK 30464 PA66 (Conditioned) Description: Impact-modified and stabilized injection- molding grade for components and housings with good low temperature impact resistance.Information provided by BASF |