Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.3 - 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.3 - 1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 0133 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Melt Flow | 1.3 - 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.3 - 1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem PH 0133 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |