Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.86 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.86 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Silon Tabond 3043 Adhesive Resin TABOND 3043 is HDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Stro.. |