Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.80 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.80 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex APEX® 130-P Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Features: Flame Retardant; Sunlight Resistant (720 hours) Uses: Flexible Cord Jacketing Forms: Pellets Wire Types: SJTW; STW; SVT; SRDT Agency Ratings: UL QMTT2.. |