Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.78 g/10 min | 1.78 g/10 min | JIS K7210 |
Stellarchem HP-930NC-HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Melt Flow | 1.78 - 27.8 g/10 min | 1.78 - 27.8 g/10 min | Average value: 9.93 g/10 min Grade Count:30 |
Overview of materials for Acetal Copolymer, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Impact Modified". Each property range of values reported is minimum and maximum values.. |