Physical Properties Metric English Comments
Melt Flow 1.21 - 37.0 g/10 min
1.21 - 37.0 g/10 min
Average value: 10.9 g/10 min Grade Count:31
Overview of materials for Polyimide
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Melt Flow 1.21 - 24.2 g/10 min
1.21 - 24.2 g/10 min
Average value: 9.36 g/10 min Grade Count:4
Overview of materials for Thermoplastic Polyimide, Unfilled