Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.97 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.97 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell SEQUEL® E5000 TPO Description: SEQUEL® E5000 thermoplastic olefinic elastomer (TPO) is designed for extrusion applications that require high mechanical stiffness, thermal stability, good low-temperature properties.. |
|||
Melt Flow | 0.97 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.97 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Arkema Group Evatane® 1005 VN 4 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for flexible films with high transparency and very high mechanical properties. Examples: high strength stretch film, greenhous.. |