Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.43 - 0.57 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.43 - 0.57 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 0.43 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.43 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
Braskem BS 002J HDPE Blow Molding Polyethylene
(discontinued **) Applications: Bottles up to 60 liters with high ESCR; bottles for surface-active agents. Information provided by Braskem |
|||
Melt Flow | 0.43 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.43 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Paxon™ EX49-006 Extrusion Grade Resin
(discontinued **) EX49-006 is an unstabilized high density polyethylene extrusion grade polyethylene copolymer. It is designed for blending and compounding with fillers, such as wood flour, to give uniform mixing an.. |
|||
Melt Flow | 0.43 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.43 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Paxon™ EA55-003 Blow Molding Resin Product Description: EA55-003 is an unstabilized blow molding grade high density polyethylene copolymer. The base resin can be compounded to incorporate such things as stabilizers, fillers, and col.. |