Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.26 - 0.42 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.26 - 0.42 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GF 4950 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 0.26 - 0.42 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.26 - 0.42 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GF 4960 HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Melt Flow | 0.24 - 0.42 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.24 - 0.42 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238-00 |
Ipiranga Petrochem GM 9450 F HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |