Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.29 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 58D HDPE Blow Molding Resin
(discontinued **) Features: Good ESCR, high stiffness, good impact strength, slightly tougher alternative to Sclair 58A.Applications: Small part blow molding, food, pharmaceuticals, HIC containers.Data provided by th.. |
|||
Melt Flow | 0.29 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 59F HDPE Blow Molding Resin
(discontinued **) Features: High impact resistance, good stiffness, moderate ESCR.Applications: Food packaging, small parts (HIC), oil bottles.Data provided by the manufacturer. |
|||
Melt Flow | 0.29 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.29 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem BS 002 HDPE Blow Molding Polyethylene
(discontinued **) Applications: Bottles for medicines, cleaning products, cosmetics, food products and surface-active agents. Information provided by Braskem |
|||
Melt Flow | 0.29 g/10 min | 0.29 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® LB832001 High Density Polyethylene ApplicationsPETROTHENE LB 8320-00 resin is designed for sheet extrusion, vacuum forming and thermoforming. This resin exhibits very low sag, high stiffness.Regulatory StatusLB 8320-00 meets the req.. |