Physical Properties Metric English Comments
Melt Flow 0.23 - 0.33 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.23 - 0.33 g/10 min

@Load 11.0 lb,
Temperature 374 °F
DIN 53735
Iran Petrochemical (PCC) Arak BL4 HDPE
Information provided by Iran Petrochemical Commercial Co.
Melt Flow 0.23 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.23 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM-D1238
Braskem GP5550 HDPE High Density Extrusion Polyethylene
GP5550 is a high-density polyethylene with high molar mass. It is produced with bimodal technology and shows excellent mechanical properties and high resistance to stress cracking. Its applications ..