Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.110 - 24.0 g/10 min | 0.110 - 24.0 g/10 min | Average value: 4.63 g/10 min Grade Count:20 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Extrusion Grade". Each property range of values reported is min.. |