Physical Properties Metric English Comments
Melt Flow 0.0800 - 150 g/10 min
0.0800 - 150 g/10 min
Average value: 11.3 g/10 min Grade Count:448
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..
Melt Flow 0.0800 - 80.0 g/10 min
0.0800 - 80.0 g/10 min
Average value: 14.7 g/10 min Grade Count:399
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..