Physical Properties Metric English Comments
Melt Flow 0.075 g/10 min
0.075 g/10 min
ASTM D1238
LyondellBasell Alathon® L4907 High Density Polyethylene
ApplicationsALATHON L 4907 is a high molecular weight high density copolymer with broad dimodal molecular weight distribution. This resin exhibits high density and stiffness and is designed for gro..