Polymer Property : Water Vapor Transmission = 4.19 g/m²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 4.19 g/m²/day

@Temperature 38.0 °C
0.270 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 26MB777 OPP Film
Product Description: A high gas barrier, biaxially oriented transparent polypropylene film, coated on one side PVdC, one side acrylic. This film provides outstanding performance on all packaging mac..
Water Vapor Transmission 4.19 g/m²/day

@Temperature 38.0 °C
0.270 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Bicor™ 32MB600 OPP Film
Product Description: A biaxially oriented transparent polypropylene film, acrylic coated two sides. Gives outstanding performance on overwrap and HFFS machines.Availability: Africa & Middle East, As..
Water Vapor Transmission 4.19 g/m²/day

@Temperature 38.0 °C
0.270 g/100 in²/day

@Temperature 100 °F
90% RH; ExxonMobil Method
ExxonMobil Oppalyte™ 40MH247 OPP Film
Product Description: A super white opaque, modified higher density, biaxially oriented polypropylene film. This opaque and stiff film is ideal for mono material requirements and it has been especial..