Polymer Property : Water Vapor Transmission = 32.2 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 500 g/m²/day

@Temperature 23.0 °C
32.2 g/100 in²/day

@Temperature 73.4 °F
50% RH; ASTM E96B
Lubrizol ESTANE® 58237 Ether Based Thermoplastic Polyurethane
Features: High moisture vapor transmission. Good physical properties and elasticity.Uses: Blown and flat die/cast film extrusion.Available in Americas, Europe, Middle East, Africa, India and AsiaInf..