Polymer Property : Water Vapor Transmission = 2.00 g/100 in²/day Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Water Vapor Transmission 31.0 g/m²/day

@Temperature 38.0 °C
2.00 g/100 in²/day

@Temperature 100 °F
90% RH, unmetallized; ASTM F1249
DuPont Teijin Films Mylar® M813 Polyester Film, 48 Gauge
Mylar® M813 is a clear, pretreated base film with high gloss, low haze, and excellent processability. It is a one side pre-treated polyester designed for improved ink adhesion and may be suitable f..